Biscaia, HC, Borba IS, Silva C, Chastre C.  2016.  A Nonlinear Analytical model to predict The full-range debonding process of FRP-to-parent material interfaces free of any mechanical anchorage devices, 15 March 2016. Composite Structures. 138:52-63. AbstractWebsite

Ever since Fibre Reinforced Polymers (FRP) began to be used in the repair or strengthening of structural elements, the premature debonding of the FRP composite from the substrate has been an important drawback that have been motive of several studies. The importance of knowing and describing the full-range behaviour of FRP-to-parent material interfaces rigorously is therefore urgent. However, at present, there are no analytical solutions that describe the full-range behaviour of such interfaces that help us to understand the full debonding phenomena of FRP-to-parent material interfaces free of any mechanical anchorage devices. Therefore, the aim of this study is to contribute the advances of that knowledge through an analytical solution by means of an exponential bond-slip model that is known to represent the nonlinearities involved in the debonding process of the FRP composite from the substrate. Analytical solutions for the slips, strains in the FRP composite, bond stress distributions along the bonded interface and stresses in the substrate are presented. A full-range load-slip analysis is also discussed.

Biscaia, H, Chastre C, Borba I, Silva C, Cruz D.  2016.  Experimental evaluation of bonding between CFRP laminates and different structural materials. Journal of Composites for Construction. 20:04015070., Number 3 AbstractWebsite

This study presents an analysis of Carbon Fiber Reinforced Polymers (CFRP)-to-parent material interfaces based on 40 single-lap shear tests intended to highlight the strength of the interfaces under fracture mode II. Three different substrates are analyzed: timber;concrete and steel, using the same CFRP laminates and adhesive agent. The Externally Bonded Reinforcement (EBR) technique was used throughout the study. The results show that the CFRP-to-timber interfaces had the highest strength but also showed that these interfaces need a longer bonded length in order to reach maximum strength, i.e., CFRP-to-timber interfaces had the longest effective bond length. The local non-linear bond-slip curve of CFRP-to-concrete can be approximated to exponential curves, whereas the CFRP-to-timber or steel interfaces showed tri-linear and bi-linear bond-slip relations, respectively. Also, the CFRP-to-timber interfaces revealed the highest fracture energy.